http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2005084486-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_03d0f52bb4069f8a19d70dcfb697c67a |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03C3-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03C1-498 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03C1-74 |
filingDate | 2003-09-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_0f635d6539a0b3a26fd4a84ad59a6d72 |
publicationDate | 2005-03-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2005084486-A |
titleOfInvention | Package of photothermographic material |
abstract | PROBLEM TO BE SOLVED To provide a package of a photothermographic material excellent in storage stability. A sheet-like laminate of a photothermographic material having an image forming layer containing at least a photosensitive silver halide, a non-photosensitive organic silver salt, a reducing agent, and a binder on one surface of a support, A package comprising the carrier of the laminate and a packaging material, wherein 1) the image forming layer has a thickness of 4 μm to 12 μm, and 2) at least a part of the image forming layer of the photothermographic material is formed. And 3) a package made of a paper material characterized in that the carrier has at least one of the following A and B: A: Paper material in which 50% by mass or more of the pulp raw material is virgin pulp, B: Paper material containing alkyl ketene dimer and cationic starch. [Selection figure] None |
priorityDate | 2003-09-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |