assignee http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_80ea019a11b415b0198345099a2642fd
classificationIPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C21D1-607
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C21D9-40
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/F16D23-06
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C22C38-00
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/F16D23-14
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B21D53-26
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C21D8-00
filingDate 2003-09-03-04:00^^<http://www.w3.org/2001/XMLSchema#date>
inventor http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b6d5243c407dffea88777b99df801f41
publicationDate 2005-03-24-04:00^^<http://www.w3.org/2001/XMLSchema#date>
publicationNumber JP-2005074502-A
titleOfInvention Method for manufacturing steel annular member
abstract PROBLEM TO BE SOLVED: To realize a manufacturing method capable of obtaining a steel annular member such as a synchronizer ring, a rolling ring for a clutch release rolling bearing unit or the like at a low cost while ensuring sufficient shape accuracy and dimensional accuracy. When a steel material is subjected to a heat treatment for quenching and then cooled, the material is rapidly cooled to 200 to 350 ° C., and then a press with a processing rate of 3% or more is applied to the material. Apply processing. Based on this press working, distortion does not easily occur in the obtained intermediate material, and it becomes easy to ensure shape accuracy and dimensional accuracy. Furthermore, after the press working, the intermediate material is cooled to a temperature below the Ms point to cause martensitic transformation. Then, the hardness of the intermediate material is increased to a required value. [Selection] Figure 1
isCitedBy http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-102401024-A
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-109385509-A
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2010002052-A
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9133894-B2
priorityDate 2003-09-03-04:00^^<http://www.w3.org/2001/XMLSchema#date>
type http://data.epo.org/linked-data/def/patent/Publication

Incoming Links

Predicate Subject
isDiscussedBy http://rdf.ncbi.nlm.nih.gov/pubchem/taxonomy/TAXID106546
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID3650774
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID428508361
http://rdf.ncbi.nlm.nih.gov/pubchem/anatomy/ANATOMYID106546

Total number of triples: 24.