http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2005068290-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_129e393582e6bdf4029baf2206522f45 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F2-00 |
filingDate | 2003-08-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c3c36e2ec85e1a1af2c2ff7ab61d4038 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ebdefe4b67d949d56a03b6a52d338ef5 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_86617ac0bc0c7d86bfc0f0a1ad1e0266 |
publicationDate | 2005-03-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2005068290-A |
titleOfInvention | Manufacturing method of resin molding |
abstract | PROBLEM TO BE SOLVED: To provide a method for producing a homogenous and thick resin molded article in order to enable mass production of homogenous precision machining members and supply precision machining members with stable machining characteristics. To do. In the production of a resin molded product in which a substrate containing a polymerization initiator is impregnated into a substrate to be impregnated and then polymerized, the impregnation is 298.15 K, the constant pressure molar heat capacity at 1 atm is 30 J / mol ยท K or more. And in a medium having a temperature not higher than 50K lower than the decomposition temperature of the polymerization initiator. [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2008111073-A |
priorityDate | 2003-08-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |