http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2005047982-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_a07d0b3e3169dd026ecd9113fc9cc4ad |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J9-12 |
filingDate | 2003-07-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9399390434f7ad139036d603b4bf6853 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5aa3a1b36eb0ad138661638a7895f136 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c02d63231f1017d59e8353eb8646e317 |
publicationDate | 2005-02-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2005047982-A |
titleOfInvention | Resin composition and high-frequency coaxial cable using the same |
abstract | The present invention provides a resin composition having good foamability and electrical characteristics. The resin composition according to the present invention comprises: Low density polyethylene with a density of 0.925 to 0.930 g / cm 3 is mixed with 55 to 95 parts by weight of medium density polyethylene or high density polyethylene of 0.931 g / cm 3 or more at a ratio of 5 to 45 parts by weight. 100 parts by weight of the mixture It is comprised with the mixed composition which mixed the foaming nucleating agent in the ratio of 0.001-0.2 weight part. In addition, the high-frequency coaxial cable 10 according to the present invention is provided with a foam insulating layer 12 made of a foam of a resin composition on the outer periphery of a conductor 11. [Selection] Figure 1 |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2011009206-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2006339099-A |
priorityDate | 2003-07-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |