http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2005029744-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_997ed5b3b186e8e8ddd4b0f8685a1d12 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G64-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G11B7-254 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02B5-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G11B7-2534 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02B1-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G11B7-257 |
filingDate | 2003-07-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_018a5b03942234a225c3498cad83c6dc |
publicationDate | 2005-02-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2005029744-A |
titleOfInvention | Polycarbonate resin pellets |
abstract | [Problem] To provide a polycarbonate resin pellet having excellent heat resistance and rigidity and having a specific range of shapes. A polycarbonate copolymer pellet in which 5 to 95 mol% of the total dihydroxy component is represented by the following general formula [1] and 95 to 5 mol% is represented by the following general formula [2]: (1) The specific viscosity of the copolymer measured under specific conditions is 0.23 to 0.45, (2) the pellets are elliptical cylinders of specific dimensions, and (3) the fine powder measured under specific conditions is 1% by weight. The following is assumed. [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2013216014-A |
priorityDate | 2003-07-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |