http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2005029593-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_ad2cd796f8c4dcb425ddcc68707d3444 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J5-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L67-00 |
filingDate | 2003-07-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b7d9ef1df99e74bdd632c7826aef6eac http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_75169bdd42220e74b25d121a768d1eeb http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b90163df660a5f973c8ccaffe3a28c0a |
publicationDate | 2005-02-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2005029593-A |
titleOfInvention | Biaxially stretched polyester resin film for twist packaging |
abstract | The present invention provides a film further provided in a polyester resin film having excellent antistatic properties such as heat resistance, moisture resistance and scent retention, paying attention to twisting, among other properties of cellophane. To do. Polyethylene terephthalate, a polyester and / or copolymer polyester having a glass transition temperature of 35 ° C. or higher and a polyester and / or copolymer polyester having a glass transition temperature of 34 ° C. or lower are mixed in a specific ratio, and A biaxially stretched polyester film having a film friction coefficient of 0.25 to 0.90. [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-2408850-A4 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2022091355-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-7029021-B1 |
priorityDate | 2003-07-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |