Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_fe53dba7cfb725b1df38f33bad74b24d |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01P2006-80 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01P2004-61 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02P10-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01P2002-88 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01P2006-40 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01G1-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C22B1-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C22B1-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01G49-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01G53-42 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01G53-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01B13-185 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C22B34-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C22B3-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01G41-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01G33-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01G25-00 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C01B13-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C01B13-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C01G53-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C01G33-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C01G41-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C01G31-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C01G25-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C01G1-02 |
filingDate |
2004-05-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_799c23681fab0d026baea157e3c68449 |
publicationDate |
2005-01-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-2005015327-A |
titleOfInvention |
Method for producing metal composite oxide |
abstract |
[PROBLEMS] To improve the reaction rate and selectivity of a solid-phase reaction and increase productivity in producing a complex oxide of a valuable metal by a solid-phase reaction between an oxide of a valuable metal and an alkali (earth) metal salt. thing. A valuable metal oxide or a substance containing the same and an alkali (earth) metal salt are co-pulverized until the particle size of the valuable metal oxide or the substance containing the same becomes a median value of 10 μm or less. The co-pulverized product is heated to a temperature of 200 ° C. or higher to cause a solid phase reaction between an oxide of a valuable metal and an alkali (earth) metal salt, and a composite oxide of the valuable metal and an alkali (earth) metal. How to manufacture. [Selection] Figure 1 |