http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2004363491-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_72400f6217740815eeb832b0d3d12e92 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01G9-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01G9-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01G9-052 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01G13-00 |
filingDate | 2003-06-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_791984863c25d248980c0f04d24cfeff http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6e4b1e00d63df1d8d294959314b3a8d2 |
publicationDate | 2004-12-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2004363491-A |
titleOfInvention | Method for manufacturing solid electrolytic capacitor |
abstract | A method of manufacturing a solid electrolytic capacitor capable of simultaneously processing a plurality of electrolytic capacitors in a plurality of main manufacturing steps is provided. According to a method for manufacturing a solid electrolytic capacitor of the present invention, a valve metal powder dispersion is applied to a base film at a predetermined interval in a substantially square shape, and one end of the valve metal dispersion application section is applied. A valve action metal foil cut into a comb shape is overlapped on the portion so that its teeth are placed, and a valve action metal powder dispersion is applied again so as to overlap the valve action metal powder dispersion application portion. Vacuum sintering of the element sheet in which the metal foil is sandwiched between the valve action metal powder dispersion coating layers to produce an anode element sheet in which a plurality of anode elements are connected, and batch-processing this anode element sheet through a holder The work efficiency can be improved by attaching the jig to the jig and performing the operations of the chemical conversion treatment, the formation of the solid electrolyte layer, the formation of the carbon layer, and the formation of the silver metal layer in units of the jig. [Selection] Fig. 10 |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-4620184-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-WO2010107011-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2006339182-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-102356442-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-111834637-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9202634-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2008098279-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2007095935-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9378897-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2010107011-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8847437-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-111681515-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9142359-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9330851-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2013074081-A |
priorityDate | 2003-06-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 53.