abstract |
An object of the present invention is to provide a softener composition for a thermoplastic elastomer, a soft thermoplastic elastomer composition, and a molded article using the same, which have excellent moisture retention and low oil bleeding feeling. A softener composition for a thermoplastic elastomer containing (a) 100 parts by weight of a softener for a non-aromatic hydrocarbon rubber, (c) 0.1 to 30 parts by weight of a surfactant, 100 parts by weight of a softener for an aromatic hydrocarbon rubber, (b) 3 to 110 parts by weight of a hydrogenated and / or partially hydrogenated block copolymer, (c) 0.1 to 30 parts by weight of a surfactant, A gel-like (jelly-like) thermoplastic having a hardness at room temperature of 40 A or less containing (d) 0.1 to 20 parts by weight of an antifoaming agent and (e) 1 to 30 parts by weight of an olefin resin, if necessary. An elastomer composition and a molded article using the same. [Selection diagram] None |