http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2004291626-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_24aca9ded2638ea793d05360dde7a4a0 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B65D65-40 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-32 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B5-22 |
filingDate | 2004-02-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_97a1403fd8119cf326673c3f421145af |
publicationDate | 2004-10-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2004291626-A |
titleOfInvention | Propylene resin multilayer foam sheet and mail box |
abstract | 【Task】 An object of the present invention is to provide a propylene-based resin multilayer foam sheet having a high expansion ratio and a beautiful appearance. [Solution] In a propylene-based resin multilayer foam sheet having a resin layer (1) and a resin layer (2) on the surface of a propylene-based resin foam layer (3) obtained by co-extrusion using a T-die, foaming of the foam layer When the magnification is 2.5 times or more, the foamed layer (3), the resin layer (1) and the resin layer (2) have a melt tension (MT (190)) at 190 ° C. and a melt flow rate (MFR) at 230 ° C. (230)) contains 10% by weight or more of the linear propylene polymer (A) satisfying MT (190) ≧ 7.52 × MFR (230) (−0.576) , and the resin layer ( A multilayer foamed sheet made of a propylene-based resin, wherein 1) and the resin layer (2) contain a filler (a). [Selection diagram] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10059037-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2017136702-A |
priorityDate | 2003-03-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 57.