http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2004287264-A

Outgoing Links

Predicate Object
assignee http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_4af0df9a26ff4aafde7285cbd8eb12f4
classificationCPCAdditional http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03H2001-2615
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G11B2007-0013
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03H2260-12
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10S359-90
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03H2001-0264
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G11B2007-0009
classificationCPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G11B7-266
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G11B7-245
classificationIPCAdditional http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G11B7-00
classificationIPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G11B7-26
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G11B7-245
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03H1-02
filingDate 2003-03-24-04:00^^<http://www.w3.org/2001/XMLSchema#date>
inventor http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8c7beb4f89ef4ee2e25ca5ca8e3da904
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4d99b3141b0db1715838c5faed53863c
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5d5ec46ae758059c0f40077481e69b5a
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_665aff6135c84f2eeac9ac0ba2bec49e
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9c5e9fc3db25d9ca14b62b3284cf8bb8
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_216b1b964d9dd3dfbb8ea1aa684ec87a
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7d50ee473bb813fcc0079a4eff1eac3a
publicationDate 2004-10-14-04:00^^<http://www.w3.org/2001/XMLSchema#date>
publicationNumber JP-2004287264-A
titleOfInvention Optical recording medium and method for manufacturing optical recording medium
abstract An optical recording medium having a thick recording layer is manufactured by using a spin coating method. A photoisomer that isomerizes on a surface of a recording layer formed by spin-coating a first coating solution containing a photoisomerization component with light having the same wavelength as the photoisomerization component contained in the recording layer. An intermediate layer is formed by spin-coating a second coating solution containing a chemical component and not dissolving the recording layer. Since the formed intermediate layer is not dissolved by the first coating liquid, a recording layer can be further laminated thereon. As a result, the thickness of the recording layer is increased and the recording density is increased. [Selection diagram] None
isCitedBy http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2010515088-A
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2007127810-A
priorityDate 2003-03-24-04:00^^<http://www.w3.org/2001/XMLSchema#date>
type http://data.epo.org/linked-data/def/patent/Publication

Incoming Links

Predicate Subject
isDiscussedBy http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID419512635
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID408299504
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID415938803
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID2272
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID962
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID408299503
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID320488

Total number of triples: 36.