http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2004285329-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_d9cb217f83556ce2a418344c2d485415 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F279-02 |
filingDate | 2004-03-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ee9f2e2a0dc2cf35cd85ebe73ea0c357 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2557ef4aadc99e092534a1cf3e5a8e50 |
publicationDate | 2004-10-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2004285329-A |
titleOfInvention | Polystyrene resin composition |
abstract | PROBLEM TO BE SOLVED: To improve the cold flow property of rubber and to simultaneously improve the reactivity with styrene monomer, impact resistance, gloss performance, tensile strength and tensile elongation performance, and low temperature properties in a well-balanced manner. Offer of things. SOLUTION: In a rubber-modified impact-resistant styrenic resin composition containing a rubber-like polymer, the rubber-like polymer is a high cis-high vinyl polybutadiene, which is obtained by being modified in the presence of a transition metal catalyst. A rubber-modified impact-resistant styrene resin composition, which is polybutadiene, and wherein the rubber particle diameter in the impact-resistant styrene resin composition is in the range of 0.8 to 3 μm. [Selection diagram] None |
priorityDate | 2003-03-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |