http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2004284899-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_3733d9a1de9624214256dc2cb7ea57fb http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_3e4d17f9d5f0e7ee9b974b0ed79614bb http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_9090aa3518bcf59d608c0363a13664f8 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2111-28 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02W30-91 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B20-12 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B20-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B14-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B28-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B14-30 |
filingDate | 2003-03-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_85e13133a614f5beafd73f1f9b2e7992 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4784ade6541421f41eddfd89582c7411 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_aca59f24a0d6ef506a3c6109450d4e68 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f8aba9cf7e4201fc5ec82fe4363ee03a http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f9e488e50b58ef7fd9c4a5abb5a7b2d3 |
publicationDate | 2004-10-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2004284899-A |
titleOfInvention | Fine aggregate for lightweight refractory concrete, method for producing the same, and method for producing lightweight refractory concrete using fine aggregate for lightweight refractory concrete |
abstract | An object of the present invention is to provide a fine aggregate for lightweight refractory concrete which is useful for producing lightweight refractory concrete excellent in fire resistance. SOLUTION: A fine aggregate having a diameter of 5 mm or less, which contains water Wi inside and is covered with surface water Wo, is obtained by removing ultrafine particles by washing ash having a small particle diameter and classification. The fine aggregate is dried at 670 to 730 ° C. to remove the surface water Wo and generate a void S in which a part of the water Wi is removed. Thereafter, heat treatment is performed at 800 to 850 ° C. to increase the ratio of the amorphous component and leave a void S containing residual moisture therein. Thereafter, the blocking process of the surface layer of the bubbles W of fine aggregate in the coating material, further increasing to viscosity by adding thereto cement and water, to the surface of the fine aggregate, OH released from the cement - pH by ion Is increased to form a film C having a high viscosity, and finally a fine aggregate having a water content of 3 to 5% by weight is obtained. [Selection diagram] Fig. 1 |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2009029655-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-114262231-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-101154427-B1 |
priorityDate | 2003-03-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 51.