http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2004268501-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_e62ede3836b2bb1ca2b837d75432c55e |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B60R13-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B25-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B7-02 |
filingDate | 2003-03-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_58c9fa94a977d849f6ce4dbab2e20064 |
publicationDate | 2004-09-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2004268501-A |
titleOfInvention | Resin laminate |
abstract | The present invention provides a resin laminate having a surface layer with high gloss and excellent flexibility and scratch resistance. A resin laminate comprising a resin substrate and a surface layer formed on the design surface side of the resin substrate, wherein the resin substrate is disposed along the surface layer, an olefin resin and an olefin elastomer. The resin is composed of one or a plurality of regions selected from the group of styrene-based elastomers, and the surface layer is made of a resin that can be composite-molded with a resin substrate and satisfy the following conditions (1) to (3): Become. (1) JIS-A hardness according to JIS K6253 is 90 or less (2) Surface gloss according to JIS Z8741 is 10% or more (3) Using a hemispherical sapphire scratch needle with a radius of 0.05 mm at the tip, a vertical load of 500 g Defect depth when the surface is scratched with 30μm or less [selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2006210905-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8426544-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8569437-B2 |
priorityDate | 2003-03-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 35.