http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2004250563-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_ca281a36dc88c033ae84728f46ecd5a3 |
classificationIPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29K21-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29L31-58 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C41-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L53-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-08 |
filingDate | 2003-02-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6ab50c74c7b4e3470da526ff0fe982b6 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_da08d055a05767a7ede9db35749c3d5d http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e4b92f66f32171d9055a2d03508c9823 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ff2e10ea9329ed05d51ef3c78adf7461 |
publicationDate | 2004-09-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2004250563-A |
titleOfInvention | Thermoplastic elastomer composition for slush molding, powder, and skin using the same |
abstract | PROBLEM TO BE SOLVED: To provide a thermoplastic elastomer composition for slush molding having good adhesion to urethane foam as a buffer layer and excellent in meltability, a powdered material thereof, and a slush molding obtained by using the powdered material. To provide an epidermis. SOLUTION: At least one polymer block A mainly composed of a vinyl aromatic hydrocarbon compound monomer unit and at least one polymer block A mainly composed of a hydrogenated butadiene monomer unit are contained in 100 parts by mass of a polypropylene resin. The polymer block B has a hydrogenation ratio of 90% or more, and the ratio of the vinyl aromatic hydrocarbon compound in the hydrogenated block copolymer is 5 to 25% by mass. And 100 parts by mass of a blend containing 20 to 500 parts by mass of a hydrogenated block copolymer having an average of 1,2 bond content of polymer block B before hydrogenation of at least 62 mol%. For slush molding, which contains 5.0 to 20 parts by mass of an olefin-based polymer having the formula (I) and a catalyst for promoting the reaction of isocyanate, and has a predetermined MFR value. In the over composition. [Selection diagram] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-4680081-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2006143942-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-WO2019026891-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2019026891-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2007211071-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-11015046-B2 |
priorityDate | 2003-02-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 61.