http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2004250466-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_9b5d58119b48e6e6ae449afc394066f3 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J5-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L67-02 |
filingDate | 2003-02-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_23543e4c031cd63e05f927fb38d1b9e0 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_862500dcb5e2e2b9794b0aaa07952bea |
publicationDate | 2004-09-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2004250466-A |
titleOfInvention | Heat-shrinkable polyester tube |
abstract | An object of the present invention is to obtain a heat-shrinkable polyester tube having excellent resistance to an electrolytic solution. A crystal is melted at a heating rate of 10 ° C./min using a differential scanning calorimeter, heated to 300 ° C., held at 300 ° C. for 1 minute, and then cooled to room temperature at a cooling rate of 10 ° C./min. (A) A heat-shrinkable polyester tube formed from a resin composition containing a polyethylene terephthalate resin as a main component and having a measured crystallization temperature of 200 ° C to 230 ° C. [Selection diagram] None |
priorityDate | 2003-02-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 107.