http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2004247152-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_d9cb217f83556ce2a418344c2d485415 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02P70-50 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-50 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M8-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-88 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M8-10 |
filingDate | 2003-02-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_13d623eb6dbf47bf7492835f58c715ae http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9f02fdd964048cd0dcd037870bcbfa6f http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5e795a4eb132b47adac31693a39b108e http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_fc671a4c7c8c1af48a2b1dd0a75dc70c |
publicationDate | 2004-09-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2004247152-A |
titleOfInvention | Electrolyte membrane-electrode assembly, fuel cell, and method for producing electrolyte membrane-electrode assembly |
abstract | An electrolyte membrane-electrode assembly which simplifies the process and has high production efficiency and can be applied to an industrial process, a fuel cell using the electrolyte membrane-electrode assembly, particularly a direct methanol fuel cell and Provided is a method for manufacturing an electrolyte membrane-electrode assembly. A catalyst layer is formed by directly applying paste for forming a catalyst layer on both sides of an electrolyte membrane, and the catalyst layer is smooth without any unevenness or cracks in the catalyst layer. A fuel cell using the electrolyte membrane-electrode assembly, a direct methanol fuel cell using the electrolyte membrane-electrode assembly, and immersing in ion-exchanged water at room temperature (25 ° C.) for 1 hour. The dimensional change rate after swelling is 0 to 3% in both the vertical and horizontal directions as compared with the dry state, and the catalyst layer forming paste is directly applied to both surfaces of the electrolyte membrane whose shape does not change. And a method for producing an electrolyte membrane-electrode assembly in which a catalyst layer is formed. [Selection diagram] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2004253336-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-7127603-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2006092926-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2020177734-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-11261542-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2011236800-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2017512226-A |
priorityDate | 2003-02-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 158.