Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_03d0f52bb4069f8a19d70dcfb697c67a |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-3492 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J5-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B23-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02B5-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L1-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B7-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02F1-13363 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C41-28 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02F1-1335 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C41-26 |
filingDate |
2003-02-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5c5730332b7aff6950882c623394d955 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6fd03b7e0c2b101a52c0b61d5f461b0e http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_fd43a258f438ac38538e8f95bc1df7d8 |
publicationDate |
2004-09-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-2004243628-A |
titleOfInvention |
Cellulose ester film, method for producing the same, optical compensation film, polarizing plate, and liquid crystal display device |
abstract |
The present invention provides a cellulose ester film having a high retardation value and excellent optical uniformity in a film plane, and a method for producing the same. Provided are an optical compensation film and a polarizing plate using a cellulose ester film having excellent properties as a support. A liquid crystal display device having good display quality using the polarizing plate is provided. A step of casting a cellulose ester solution containing 0.01 to 20 parts by mass of a specific compound having a triazine skeleton having a planar structure as a retardation increasing agent with respect to 100 parts by mass of a cellulose ester, and drying before peeling A method for producing a cellulose ester film comprising a step of drying for 10 seconds to 90 seconds in a substantially air-free period, a cellulose ester film obtained by this method, an optical compensation film using the film, and A polarizing plate and a liquid crystal display device including these functional films. [Selection figure] None |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-7955666-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-5062261-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2011073007-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2009044471-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2009265597-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-7569261-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2014109350-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-4546370-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8017199-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2007077360-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8465673-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2006064967-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2007030466-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2007023124-A |
priorityDate |
2003-02-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |