Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_81bcff8994a4265bce4cd8ea523f682c http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_52a65b677bbedbe7bf090dd556a7cc43 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F4-64 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F4-6592 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F210-16 |
filingDate |
2003-02-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_73a201c369bc97b79f0f71b8b7bb8504 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_0dfdf7c1ca5b6a2bbd747275c66d966a http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e78cf7ad5f8400513505e72ce57c28b8 |
publicationDate |
2004-08-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-2004238496-A |
titleOfInvention |
Method for producing propylene / ethylene copolymer |
abstract |
An object of the present invention is to provide a method for producing a propylene / ethylene copolymer with high polymerization activity using an olefin polymerization catalyst containing a metallocene compound. An olefin polymerization catalyst containing titanium, zirconium, or hafnium as a transition metal and having a structure having no plane of symmetry containing the transition metal is used, and a polymerization temperature of 50 to 150 ° C. A method for producing a propylene / ethylene copolymer having a content of ethylene units in the copolymer of 0.1 to 50 mol% and an intrinsic viscosity of 2 to 12 dl / g in the above range. [Selection diagram] None |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2008101034-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2013001737-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2011126813-A |
priorityDate |
2003-02-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |