http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2004238468-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_efbfdc7316d3b1b7ceaee5366a61b6e0 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-13 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L9-00 |
filingDate | 2003-02-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_80061ca32827b68ae516eee3b6c7c6c9 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f40f803a240a7d3c015349ff4f7c9ad9 |
publicationDate | 2004-08-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2004238468-A |
titleOfInvention | Rubber composition and rubber product |
abstract | The present invention does not use natural rubber containing an allergic component, and is therefore suitable for use in direct contact with the skin. In addition, the vulcanized molded article has properties close to the elastic properties of human skin, and weather resistance. And a rubber product obtained by vulcanizing and molding the rubber composition. A rubber composition containing synthetic IR and EPDM as rubber components. EPDM content in the rubber component is 50% by weight or less. EPDM has a diene component content of 6% by weight or more. A rubber product obtained by vulcanizing this rubber composition, wherein the tensile stress M 200 at the time of 200% elongation is 15 kgf / cm 2 (14.7 × 10 5 Pa) or less, and the tensile strength ratio M 200 / M 100 , M300 / M200 , and the rubber product whose M400 / M300 are all 2.0 or less. [Selection diagram] Fig. 1 |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2017507202-A |
priorityDate | 2003-02-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 53.