http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2004204011-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_24aca9ded2638ea793d05360dde7a4a0 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F8-50 |
filingDate | 2002-12-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_58b54eaba7e4f1be8e6a0ede89ac6c88 |
publicationDate | 2004-07-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2004204011-A |
titleOfInvention | Method for producing olefin resin |
abstract | An object of the present invention is to provide a method for economically producing an olefin resin having desired fluidity and excellent flexibility. An olefin-based resin obtained by heat-treating the component (A) at a heat treatment temperature of 210 to 300 ° C. in the presence of 0.01 to 10 parts by weight of the following component (B) based on 100 parts by weight of the following component (A): Production method. (A): an amorphous α-olefin-based resin (a1) comprising the following components (a1) and / or (a2): an amorphous α-olefin copolymer (a2) comprising two or more α-olefin units Amorphous ethylene-α-olefin copolymer (B) consisting of ethylene and two or more α-olefin units: peroxide [selection diagram] None |
priorityDate | 2002-12-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |