http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2004149590-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_1374dd16777534b65ad4422333245af8 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J3-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L79-08 |
filingDate | 2002-10-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_73a5165336b5b70a9dacd6ae87567a2a http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_79a37a9fcae684a2753b4f26a87a3dd5 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_cb1c93733d0131c1c6ae9b534471aef8 |
publicationDate | 2004-05-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2004149590-A |
titleOfInvention | Aromatic polyamic acid solution with enhanced stability and method for producing the same |
abstract | An object of the present invention is to provide a method for producing a stable polyamic acid solution suitable as a precursor for producing a molded product such as an aromatic polyimide fiber or film. A azeotropic solvent with water is added to a solution of an aromatic polyamic acid maintained at a temperature of 30 ° C. or lower and mixed. To 150 ° C., and the mixture is stirred and mixed while removing water in the system by distillation under reduced pressure. [Selection diagram] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2016518511-A |
priorityDate | 2002-10-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 52.