http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2004143379-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_9e1bf06f55de84b78abc9a057807f7eb |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L67-02 |
filingDate | 2002-10-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3e85936534784b41f340a8c830b7c308 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a7c17fcd701d18ce95a1e29109530815 |
publicationDate | 2004-05-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2004143379-A |
titleOfInvention | Aqueous resin dispersion |
abstract | [PROBLEMS] To form a resin film excellent in thick coating and adhesion even when formed at a low temperature, and excellent in wettability to a substrate, and excellent in blocking resistance and solvent resistance. It is an object of the present invention to provide a resin aqueous dispersion which can be produced and has a reduced organic solvent content. A polyester resin having an acid value of 8 to 40 mg KOH / g, a weight average molecular weight of 9000 or more, and a glass transition temperature of 50 ° C. or more, a glass transition temperature of 70 ° C. or more, and a breaking elongation of 250% or less. A resin characterized by containing a polyurethane resin in a range of (polyurethane resin) / (polyester resin) = 1/99 to 30/70 (mass ratio), and having an organic solvent content of 3% by mass or less. Aqueous dispersion. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2010131767-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2014525858-A |
priorityDate | 2002-10-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 202.