Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_1af8df51ce24ca931ae718fb747f6aa0 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03G9-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03G9-087 |
filingDate |
2003-09-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6f07a8c788959e0a94dde5c8ae0c379f http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c4466f51589999a3ff203543d92668f2 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_225d89510c9a4e02a63c3bff2342e801 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ec07deb1b7a52c52709dae6062c41c82 |
publicationDate |
2004-04-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-2004126575-A |
titleOfInvention |
Developer |
abstract |
PROBLEM TO BE SOLVED: To provide a developer capable of obtaining a good image without causing charging failure even when the developer is repeatedly used for a long period of time. SOLUTION: In a developer having at least a binder particle and a coloring agent and at least an inorganic fine powder and a conductive fine powder, a volume average particle diameter Da of the conductive fine powder and The number average particle diameter Db of the primary particles satisfies the expression (1), Da ≧ 10Db (1) The release rate a of the conductive fine powder is 40% to 95%, and the release rate b of the inorganic fine powder is 0.1% to 5%. [Selection diagram] None |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2013092597-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2007248666-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2007004088-A |
priorityDate |
2002-09-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |