abstract |
An object of the present invention is to provide a polyamide composition having excellent flame retardancy, strength, heat resistance, and fluidity. A semi-aromatic polyamide (A) having a melting point of 270 ° C to 340 ° C with respect to 100 parts by weight. And the following chemical formulas (1) and / or (2) Embedded image , A molecular weight in the range of 300 to 3000, and a midpoint temperature in a thermogravimetric analysis curve measured under a nitrogen atmosphere (however, when there are a plurality of midpoint temperatures, the lowest temperature Is a polyamide composition comprising 0.1 to 10 parts by weight of a compound (B) having a temperature of 350 ° C. or higher and 1 to 100 parts by weight of a brominated flame retardant (C). [Selection diagram] None |