http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2004100081-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_ad2cd796f8c4dcb425ddcc68707d3444 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D02G3-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D02G3-48 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D06M13-335 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01F6-74 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B60C9-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D07B1-02 |
filingDate | 2002-09-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8f6e293667fa6dba24e5c193698dd8c3 |
publicationDate | 2004-04-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2004100081-A |
titleOfInvention | Polybenzazole fiber cord for rubber reinforcement |
abstract | An object of the present invention is to provide a rubber reinforcing cord having a small decrease in strength even when exposed to high temperature and high humidity for a long time. A polybenzazole fiber containing a monomer of a basic organic compound such as p-phenylenediamine, m-phenylenediamine, or a mixture thereof, or a condensate thereof is twisted to form an atmosphere at a temperature of 80 ° C. and a relative humidity of 80%. A polybenzazole fiber cord for rubber reinforcement having a tensile strength retention of 70% or more after being exposed to light for 700 hours. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2010099897-A |
priorityDate | 2002-09-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 50.