http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2004094128-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_03d0f52bb4069f8a19d70dcfb697c67a |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03C2200-43 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03C1-49881 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03C1-498 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03D13-00 |
filingDate | 2002-09-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_25bfaeedb6211510102afd250a09eea1 |
publicationDate | 2004-03-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2004094128-A |
titleOfInvention | Thermal development method |
abstract | The present invention provides a thermal development method in which density is more stable and printing time can be shortened. In a heat development method in which light development or heat development is applied to a heat development photosensitive material or a heat development recording material including a light and heat sensitive recording material, the target temperature of the heater is set higher than usual immediately after the heat development apparatus is started. It was made to raise, and after that, the raising width was decreased with time. [Selection] Figure 8 |