http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2004085773-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_24aca9ded2638ea793d05360dde7a4a0 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09B11-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02B5-223 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03F7-0007 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03F7-033 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03F7-032 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03F7-027 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02F1-1335 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02B5-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02B5-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05D1-40 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03F7-004 |
filingDate | 2002-08-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_74879ca17b7dbe6daa3a76227a8dc324 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a144f3526dc1d67cb5c2c69f8714bf36 |
publicationDate | 2004-03-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2004085773-A |
titleOfInvention | Colored photosensitive resin composition |
abstract | An object of the present invention is to provide a colored photosensitive resin composition having good coatability even when a liquid-saving coater is used. A colored photosensitive resin composition comprising (A) a colorant, (B) a binder resin, (C) a photopolymerizable compound, (D) a photopolymerization initiator, (E) a solvent, and (F) a surfactant. The surfactant, comprising (F) a surfactant in an amount of 0.0005 to 0.14 parts by mass per 100 parts by mass of the colored photosensitive resin composition excluding the surfactant; The colored photosensitive resin composition is filled into a clean glass cylindrical brown bottle having a capacity of 30 mL (height: 65 mm, diameter: 33 mm) with a capacity of 15 mL, and the colored photosensitive resin composition is filled with 15 mL of the colored photosensitive resin composition. A colored photosensitive resin in which a rotor (total length: 20 mm, diameter: 6.5 mm) is put therein, stirred by a magnetic stirrer at a speed of 700 rpm for 60 seconds, and then left for 600 seconds to be defoamed. Composition. [Selection diagram] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-4502784-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-7766530-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2006023696-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2008096782-A1 |
priorityDate | 2002-08-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 739.