http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2004025837-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_997ed5b3b186e8e8ddd4b0f8685a1d12 |
classificationIPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29K69-00 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J3-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29B9-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G11B7-26 |
filingDate | 2003-03-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_1940ffef2577342028a25b89a9daa434 |
publicationDate | 2004-01-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2004025837-A |
titleOfInvention | Method for producing aromatic polycarbonate resin pellets |
abstract | An object of the present invention is to provide a method for producing an aromatic polycarbonate resin pellet which has a small amount of fine powder and is suitable as an optical molding material. A method for producing a pellet as an optical molding material by melt-extruding an aromatic polycarbonate resin into a strand, cooling and cutting the same with warm water, and (1) uniformly extruding the extruded strand around the strand. (2) The strand is cut at a temperature such that the pellet temperature immediately after cutting the strand is 110 to 130 ° C. [Selection diagram] None |
priorityDate | 1998-04-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 150.