http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2004018902-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_9e1bf06f55de84b78abc9a057807f7eb |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C23C22-07 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C23C28-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C23C22-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05D7-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05D7-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C23C22-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B15-082 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B15-08 |
filingDate | 2002-06-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4be2b3deb90c76e99bc6c35f0f80700a http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ed316a11bf6837085241464098eea249 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6c5f978d1c0a97c628bcaf1d0061ede8 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_46b138c2d44098fc5f53ceb7b79e0b4f |
publicationDate | 2004-01-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2004018902-A |
titleOfInvention | Rust prevention coating agent and laminated metal material |
abstract | [Object] To provide a rust-preventive coating agent which does not contain chromium and exhibits excellent rust-preventive properties, hardness and solvent resistance by short-time heat treatment. A compound (A) having two or more hydroxyl groups in a molecule, a compound (B) in which at least one carboxyl group is bonded to each of three or more consecutive carbon atoms in a molecule, and a compound It contains a basic compound (C) in an amount of 0.1 to 50 mol% with respect to the carboxyl group in (B) and an aqueous solvent (D), and the mass ratio of the compound (A) to the compound (B) is 95 / A rust-preventive coating agent characterized by being 5 to 10/90. Further, a coating formed by removing the aqueous solvent (D) from the rust preventive coating agent is provided on the surface of the metal material, and the weight loss of this coating when immersed in hot water at 60 ° C. for 30 minutes is reduced. 5% or less of the laminated metal material. [Selection diagram] None |