http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2004013061-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_cdd94f212dc7aef02fc1dcf28fa9b4fd |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02B3-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02B1-115 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02B1-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02B1-11 |
filingDate | 2002-06-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8c892eef1e5c0b383f98070b5e9eb669 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c0d6f8f5d758d6fbdc6350b715401f22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c56afe3124a90ce2da1f9eafcc1fefb4 |
publicationDate | 2004-01-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2004013061-A |
titleOfInvention | Method for manufacturing optical component and bonded element |
abstract | 【Task】 An optical component manufacturing method capable of achieving downsizing and manufacturing a high quality optical component despite maintaining high adhesion and strength of a coated film with respect to an optical component obtained by bonding a plurality of elements, And a bonded element manufactured thereby. [Solution] Since an optical component is manufactured by bonding at least two members 1 and 2 and then performing a coating process, a so-called “grasping margin” is compared with a case where each of the members 1 ′ and 2 ′ is coated. Is not provided for each of the optical components, so that the size of the optical component is reduced. In addition, if the coating surface is damaged after the parts 1 and 2 are bonded to each other, it is not necessary to separate the coating surface again in order to correct the damage, and the time and effort for manufacturing can be saved. Furthermore, since the coating process of the entire optical component can be performed at one time, when the coating process is performed on each of the components 1 and 2 individually, it is noticed that the coating has a different color for the first time when they are combined. And other problems can be avoided. [Selection diagram] Fig. 1 |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-5250851-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2006084887-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-109781262-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-11681212-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-4501065-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2008149631-A1 |
priorityDate | 2002-06-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 201.