http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2003335882-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_2cb72657cf0479385a9b5e655af1e16f |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L25-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J9-04 |
filingDate | 2002-05-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2562cdb5f4b64900719df88f0cbf5fd3 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_09c33e39a126170e0d74e57051314611 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_60a78a363fab287de246f8e409bb7a52 |
publicationDate | 2003-11-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2003335882-A |
titleOfInvention | Solvent-resistant styrenic resin composition and foam molded product |
abstract | (57) [Problem] To provide a styrenic resin composition and a foam molded article which can be reduced in cost and have improved solvent resistance. SOLUTION: It comprises the following components (A) and (B): A solvent-resistant styrene resin composition having a relative crystallinity of less than 30%. (A) Styrenic polymer 97 having an atactic structure (B) 3 to 60% by weight of a styrene polymer having a syndiotactic structure A foam molded article obtained by foaming the styrene resin composition has high solvent resistance, and the cost is reduced by weight reduction. . The weight reduction rate is preferably 3 to 80% by weight. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2010265400-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2010254930-A |
priorityDate | 2002-05-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 133.