http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2003334904-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_ad2cd796f8c4dcb425ddcc68707d3444 |
classificationIPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29K25-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29L7-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29L9-00 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C55-02 |
filingDate | 2002-05-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_76396800c82b6f14876491ac4b33c4c3 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7416b5826b0b2e65598e13d25a0b0e65 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a4471a9525f711dbf0a95e4978e1844d http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_50fa3b8c996a4e1d47109a5a9221b840 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_93cd2130d0e054a2d95aaa3688395594 |
publicationDate | 2003-11-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2003334904-A |
titleOfInvention | Easy adhesion syndiotactic polystyrene-based stretched film |
abstract | PROBLEM TO BE SOLVED: To provide an easy-adhesion syndiotactic polystyrene system having excellent adhesion between a film and an adhesive property-modifying layer, and excellent economical efficiency, recyclability, and environmental compatibility at the time of production. It is intended to provide a stretched film. SOLUTION: At least one surface of a stretched film made of a styrenic polymer having a syndiotactic structure, An adhesion modifying layer composed of a water-dispersible linear polyester satisfying the following (a) is laminated. (A) Chemical shift 1.0 ppm measured by proton NMR The ratio of B / (A + B) calculated from the integrated value A of protons at ~ 6.0 ppm and the integrated value B of protons at 7.0 ppm to 9.0 ppm is 0.07 to 0.25. In particular, after applying the aqueous dispersion of the copolymerized polyester to an unstretched film or a uniaxially stretched film, and then stretching the adhesive modified layer once or more in a uniaxial or biaxial direction, it may be formed by heat treatment. preferable. |
priorityDate | 2002-05-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 69.