http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2003327714-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_6c8d4dc7bd1a30d8fda907fceaeb4e69 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_27aa3092499b93e3144b5053272698ca |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K7-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K7-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L69-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L101-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J5-00 |
filingDate | 2002-05-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_1b1a0de3ef4e1be0ef6fed18c4c9af7e http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_1d73aa54db47f91882c0d0d8b8875a72 |
publicationDate | 2003-11-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2003327714-A |
titleOfInvention | Painted products |
abstract | (57) [Problem] To provide a coated molded article formed from a polycarbonate resin composition having excellent mechanical strength and dimensional stability and excellent adhesion of a coating film. SOLUTION: The polycarbonate is obtained by a melt transesterification method and has a temperature of 250 ° C. and an angular velocity of 10 rad /. loss angle δ and complex viscosity η * (Pa S) is a painted molded article obtained by painting a molded article of a resin composition in which 3 to 200 parts by weight of an inorganic filler is blended with 100 parts by weight of a polycarbonate satisfying the following relational expression (1). ## EQU1 ## 2500 ≦ Tan δ / η * −0.87 ≦ 6000 ° (1) |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2008208335-A |
priorityDate | 2002-05-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |