http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2003320540-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_02cfb0f1aa2718c61bdf184d53adfe79 |
classificationIPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29L11-00 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C03C17-42 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02B3-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C39-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C39-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02B5-18 |
filingDate | 2002-05-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_90f98fc9c8222e085424fc9bfef6be76 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_11ab4a7bbed3adcc6a9f9d5a81aa6dfb |
publicationDate | 2003-11-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2003320540-A |
titleOfInvention | Optical element manufacturing method |
abstract | (57) [Problem] To provide a method for manufacturing an optical element which stabilizes adhesion between resin layers and has excellent environmental resistance. SOLUTION: A silane coupling agent is applied to the entire surface of a base material 1 by spin coating and baked to form a primer layer 4. The base material and the mold having a lattice shape are brought close to each other, and the gap is filled with the uncured first layer resin 2. In this state, ultraviolet rays are irradiated for 2 minutes through the base material to cure the first resin layer 2 and then release it. An uncured second-layer resin 3 is further dropped thereon, molded in the vicinity of a mold, and then cured by ultraviolet rays similarly to the first-layer to release the mold. The outer diameter of the second resin layer 3 is larger than the outer diameter of the first resin layer 2, and the second resin layer 3 adheres to the primer layer 4 over the entire circumference. Therefore, the second resin layer is also strongly bonded to the base material 1. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2010078860-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2007145263-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2012220899-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2008001706-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-7957063-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-4932837-B2 |
priorityDate | 2002-05-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 30.