http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2003316077-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_8fb9f44db08d1c42a53f3d28eaae416f |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03G9-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03G9-09 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03G9-087 |
filingDate | 2002-04-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4e25fe1b5e71fe37d663553987de7250 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d0688e95f57a3364f3f00d4e021cada0 |
publicationDate | 2003-11-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2003316077-A |
titleOfInvention | Manufacturing method of toner |
abstract | (57) Abstract: A kneaded material containing a large amount of a release agent can be melt-kneaded using an open roll kneader without causing problems such as sagging of the kneaded material. And a method for producing a toner which is excellent in dispersibility of a colorant and can be suitably used for oilless fixing. A method for producing a toner comprising a step of melting and kneading at least a binder resin, a colorant, and a release agent using an open roll kneader, wherein the colorant is represented by the formula (I): ] Wherein the release agent contains a hydroxy acid ester, and the total content of the compound represented by the formula (I) and the release agent is 7.5 in the toner. To 30% by weight. |
priorityDate | 2002-04-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |