Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_1374dd16777534b65ad4422333245af8 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G63-18 |
filingDate |
2002-04-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7c4d7f846a8b8488a16927b9d4c8f5ed http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8f39e76752d0043958f14fa0830fce46 |
publicationDate |
2003-10-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-2003301034-A |
titleOfInvention |
Method for producing polyarylate |
abstract |
(57) [Summary] [PROBLEMS] To suitably produce a high heat-resistant polyarylate by a method with reduced equipment load. SOLUTION: The melting point is 50 ° C. or less and the boiling point is 3 at normal pressure. An aromatic carboxylic acid derivative and an aromatic hydroxy derivative are polymerized in the presence of an imide compound at a temperature of 00 ° C. or higher to obtain a polyarylate. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20160079764-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2009124961-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-102185023-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2005255990-A |
priorityDate |
2002-04-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |