Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_afea2aa6f1f892c1456cf7d7a8bc0242 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D03D15-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01F6-92 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G81-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J5-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G63-91 |
filingDate |
2002-04-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_47ae6f395a88a465c629131846be9201 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_0af2b081fe7f919e87359e74fe976065 |
publicationDate |
2003-10-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-2003292602-A |
titleOfInvention |
Polyester resin composition |
abstract |
(57) [Summary] [PROBLEMS] To improve the hydrolysis resistance (heat aging resistance) and stretching properties of polyester without significantly increasing the melt viscosity. SOLUTION: The thermoplastic polyester resin 90 to 99. A mixture containing 9% by weight and 0.1 to 10% by weight of liquid polybutene having an epoxy group at the end is melt-kneaded to block the terminal carboxyl groups of the polyester and simultaneously introduce polybutylene chains. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-7977429-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-4643226-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2006022318-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2007002180-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2005073282-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-100745560-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2006131674-A |
priorityDate |
2002-04-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |