http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2003280126-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_03d0f52bb4069f8a19d70dcfb697c67a |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03C1-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03C1-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03C1-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03C1-015 |
filingDate | 2002-09-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_59aebb013ba3d57661f7589ac0f707e0 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c72f347909feea5b65c93a3c25832d78 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_721d307d8c19624167742fb75a9b7d0e http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5efc838c87642213fe9865e9a7157b9a http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_708cf91d2801e8d2fdb0dfe6efd5e86c |
publicationDate | 2003-10-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2003280126-A |
titleOfInvention | Method and apparatus for producing silver halide photographic emulsion |
abstract | (57) [Problem] To provide uniform emulsion performance by causing a uniform chemical reaction in a processing solution. In addition, it is possible to scale up from a small-scale production system for experimental equipment to a production equipment with an optimum production scale. At least one treatment in a nucleation treatment, a nucleation growth treatment, a chemical sensitization treatment or a spectral sensitization treatment for producing a silver halide photographic emulsion is processed by a microreactor 30, 34, 38 or 50. . The micro-reactor 30, 34, 38 or 50 fine regions are used to accurately perform the nucleation reaction. The conditions for the reaction of the newly supplied silver halide nuclei with the host grains are made uniform to allow uniform growth. A sensitizing treatment is performed by doping a predetermined amount of each molecule for chemical sensitization into each crystal lattice of silver halide nuclei. Alternatively, the spectral sensitization treatment for uniformly adsorbing the molecules of the spectral sensitizer on the surface of the silver halide nuclei is performed reliably. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2007307440-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2008530505-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2011020004-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2008522806-A |
priorityDate | 2002-01-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 49.