abstract |
(57) [PROBLEMS] To provide an active matrix display device capable of forming an active element with a high yield using a lightweight plastic substrate and a method of manufacturing the same. SOLUTION: The present invention provides a plastic substrate and a glass transition temperature of 3 provided in a pixel region on the plastic substrate. A first adhesive layer having a temperature of 0 ° C. or more and 80 ° C. or less, and a glass transition temperature provided in a peripheral region around a pixel region on a plastic substrate, wherein the glass transition temperature is 10 ° C. or more higher than the glass transition temperature of the first adhesive layer; A second adhesive layer having a temperature of 200 ° C. or lower, a thin glass layer provided on the first adhesive layer and the second adhesive layer with a thickness of 150 μm or less, and an active layer provided for each pixel on the thin glass layer. Provided is a display device, comprising: a device, a display portion provided on a thin glass layer, driven by an active device, and capable of displaying each pixel, and a counter substrate provided on the display portion. |