http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2003277116-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_424db9d56b06a23aed410fcf5df652f3 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2111-00129 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2111-12 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B24-383 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B28-04 |
classificationIPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B103-44 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B28B3-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B14-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B28-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B28-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B24-38 |
filingDate | 2002-03-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_43b4ae6896823fde75d353c0e3bb9034 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_dff402f7b278d8d0b139642872e12022 |
publicationDate | 2003-10-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2003277116-A |
titleOfInvention | Method for selecting admixture, hydraulic composition for extrusion molding and admixture |
abstract | (57) Abstract: To a mixture of 90 parts by weight of cordierite, 10 parts by weight of ordinary Portland cement and 33 parts by weight of water, immediately after adding 3 parts by weight of a nonionic water-soluble cellulose ether, at 20 ° C. and 20 rpm. The admixture for a hydraulic composition for extrusion molding comprising a nonionic water-soluble cellulose ether, wherein the time when the maximum value of the torque value (torque peak) when kneaded is within 180 seconds from immediately after the addition. The admixture for the hydraulic composition for extrusion molding of the present invention can be kneaded in a short time, and at a predetermined addition amount, A uniform kneaded material can be obtained, and a smooth kneaded material for extrusion molding can be obtained. |