http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2003268176-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_24aca9ded2638ea793d05360dde7a4a0 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-098 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J5-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-134 |
filingDate | 2002-03-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_618b3d622a53d704e655759990e4a946 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_0c610c3e09d4c814b6f24693ff8bb2c5 |
publicationDate | 2003-09-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2003268176-A |
titleOfInvention | Polypropylene resin composition |
abstract | PROBLEM TO BE SOLVED: To provide a polypropylene resin composition having high rigidity, excellent color tone and excellent stain resistance of a processing machine, and a molded article comprising the same. SOLUTION: For (A) 100 parts by weight of a polypropylene resin, (B) an alkaline earth metal hydroxide 0.0 02 to 0.1 parts by weight and (C) a metal salt of carboxylic acid. A polypropylene resin composition containing 001 to 0.5 parts by weight and (D) 0.01 to 0.5 parts by weight of a phenolic antioxidant. Preferably, the polypropylene resin composition according to the above, wherein (D) the phenolic antioxidant is a phenolic compound having at least one group represented by the following general formula (I). A molded article comprising the polypropylene resin composition described above. |
priorityDate | 2002-03-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 160.