http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2003253159-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_5aeb0be4de279ad87517babcaf5e1634 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D4-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B42D15-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J5-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J7-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J201-00 |
filingDate | 2002-02-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b14dec0bc333850cd25f0c210e8e59f0 |
publicationDate | 2003-09-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2003253159-A |
titleOfInvention | Adhesive receiving layer forming ink and adhesive sheet using the same |
abstract | PROBLEM TO BE SOLVED: To provide excellent adhesiveness between an adhesive receiving layer formed on a base material and an adhesive and to obtain a high adhesive strength, so that there is no problem of peeling off at an adhesive interface during use of the product. Provided are an ink for forming an adhesive receiving layer, which can easily form an adhesive receiving layer having excellent printing ink suitability, and an adhesive sheet using the same. SOLUTION: An ink for forming an adhesive receiving layer is used, which contains a vehicle containing an acrylic photocurable component as a main component and having a volume shrinkage of 10 to 25%. Further, it is preferable to mix fine particles. The problem can be solved by an adhesive sheet in which an adhesive receiving layer is formed using a predetermined portion of at least one surface of a base material using this ink. |