http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2003246160-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_03d0f52bb4069f8a19d70dcfb697c67a |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03F7-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C25D11-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03F7-09 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C25D11-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C25F3-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B41N3-03 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B41N1-08 |
filingDate | 2002-02-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c19c2335ba2dfc868e02b4e44b0f1b36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_79318b45e514ef37f34cc1b08dc226dc http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5964d861b26a8a4d16c43918d4083ca7 |
publicationDate | 2003-09-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2003246160-A |
titleOfInvention | Method for producing aluminum support for lithographic printing plate |
abstract | (57) [Summary] [Problem] A low-purity aluminum rolled sheet (aluminum sheet containing a lot of alloy components or an aluminum sheet not prepared with alloy components) can be used. First, the provision of a method for producing an aluminum support for a lithographic printing plate that can achieve both printing durability and printing performance (dirt performance) when used as a lithographic printing plate. SOLUTION: In order, aluminum plate is 1) ratio of electricity quantity Qa at the time of anode and electricity quantity Qc at the time of cathode of alternating current aluminum plate in nitric acid aqueous solution, condition that Qc / Qa is 0.9 to 1.0 2) 1-10 g of hydrochloric acid 1 mL of aluminum chloride hexahydrate in an aqueous solution containing / L In a hydrochloric acid aqueous solution added at a rate of 0 to 70 g / L and having an aluminum ion concentration of 1 to 8 g / L, the Qc / Qa A method for producing an aluminum support for a lithographic printing plate, characterized in that the surface is electrochemically roughened under a condition of 0.9 to 1.0, and 3) anodized. |
priorityDate | 2002-02-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 257.