http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2003239146-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_1374dd16777534b65ad4422333245af8 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D02G1-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D02G3-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D03D27-00 |
filingDate | 2002-02-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6b3c9054c7942c055768199407c44d87 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_68b62ac057a6197af3c35b0d8540c50e |
publicationDate | 2003-08-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2003239146-A |
titleOfInvention | Polyester composite false twisted yarn for cut pile woven or knitted fabric and method for producing the same |
abstract | PROBLEM TO BE SOLVED: To provide a polyester false-twisted yarn which realizes an excellent color-dyed heat-dyed tone (coarse heat) and a soft and excellent napping property for a cut pile woven or knitted fabric, and a method for stably producing the same. I do. SOLUTION: A yarn group A made of polyester which is dyeable to an ionic dye and a yarn group B made of polyester which is unstainable to an ionic dye and contains 1.0 to 3.5% by weight of titanium oxide. It has a crimp rate of 1 to 4% and a total fineness of 1 20 to 250 dtex and single yarn fineness is 1 to 5 dtex Of polyester false twisted yarn. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2007056407-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-104562248-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-100395092-C http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2008025043-A |
priorityDate | 2002-02-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 29.