http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2003233150-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_03d0f52bb4069f8a19d70dcfb697c67a |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03C1-498 |
filingDate | 2002-02-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c1fef7c760fc1e2ee4c255680342f7fa http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_77d0592288a3b52e157a1c227fbea5f9 |
publicationDate | 2003-08-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2003233150-A |
titleOfInvention | Photothermographic material |
abstract | (57) [Problem] To provide a photothermographic material excellent in image storability. [Solution] At least photosensitive silver halide, non-photosensitive organic silver salt, silver on one side of a support. A photothermographic material containing a reducing agent for ions and a binder, wherein the binder contains a polymer latex in which at least one monomer containing an acid group is copolymerized, and a monomer containing a remaining acid group Is a photothermographic material, characterized in that is 0.03% by mass or less based on the total amount of the binder. |