http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2003226760-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_d93502a23a72b56472bc75854cfe7c60 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J5-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F297-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01L21-68 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01L21-673 |
filingDate | 2002-02-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_55c22f997810e59aa3a164644ea41da0 |
publicationDate | 2003-08-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2003226760-A |
titleOfInvention | Molded body |
abstract | (57) [Summary] [PROBLEMS] To maintain the sealing performance even when repeatedly used as a sealing material for a closed container or the like by pressurization, to prevent the molded articles from blocking each other, and to prevent the release of an organic substance gas. To provide a molded product that does not contaminate. SOLUTION: A polymer block [A] containing 70% by weight or more of a repeating unit derived from vinylcyclohexa, and a polymer block [B] containing 30% by weight or more of a repeating unit derived from a chain vinyl monomer, Polymer block [A]: polymer block [B] = 10: 90 by weight ratio The block copolymer having a ratio of 80:20 is molded so that the ten-point average roughness of the surface is 5 to 100 μm. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2007116904-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-101045126-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-101045184-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-3825133-A2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-3907084-A1 |
priorityDate | 2002-02-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 144.