http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2003212633-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_2c20b173ea0140e62192c70f419f5397 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02W30-91 |
classificationIPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B111-40 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B111-72 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B28-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/E04C2-26 |
filingDate | 2002-01-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_71ea325ab05031416013cfa696d5cf4f |
publicationDate | 2003-07-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2003212633-A |
titleOfInvention | Architectural molded plate, its manufacturing method and its construction method |
abstract | (57) [Problem] To provide an inexpensive, hydrophobic, heat-insulating, lightweight, water-permeable, and rigid earth-based architectural molded plate improved from a traditional plastering method, a method for producing the same, and The construction method is provided. SOLUTION: The molded plate for building is made of a first material made of lightweight aggregate. A first base material including a granule portion and a stucco portion of a main material and clay, masago soil, and a second main material mainly composed of sand, and a cement added to the first base material as an external part, A base material having a diluted water glass, a hardening agent for diluted water glass, and a second base material containing bitterness, and a reinforcing bar, a steel net, and a chemical fiber net for reinforcing the base material; It consists of a reinforcing material, is formed by filling a base material in a mold, then arranging a reinforcing material and further filling a base material, providing joints at predetermined intervals and arranging joints at joints. It is constructed by adjusting the depth and filling the filler. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2018178679-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2007246291-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2009275450-A |
priorityDate | 2002-01-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 39.