http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2003205468-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_d8a482321002bc839b45be1ca4205820 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_e32354b00edc690b0d620f2c23c32c69 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B24D3-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B24D3-34 |
filingDate | 2002-01-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_98421cb2688a5b641cd3940a418a1d43 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7cb5534ae67ea3121701f16ce2f92df7 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9bf984d532d8f9dd34c73d64c6b0d92f http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3af3feabdcdb0573998c9c4195a27ac3 |
publicationDate | 2003-07-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2003205468-A |
titleOfInvention | Conductive whetstone and method of manufacturing the same |
abstract | (57) [Summary] [PROBLEMS] To achieve high conductivity and to easily prevent metal elements from being mixed into the surface of an object to be polished, and to easily perform extremely accurate grinding and polishing. And a method of manufacturing the same. SOLUTION: A conductive grindstone 1 is made of a sintered body of inorganic abrasive grains 2 containing at least one kind of abrasive grains 4 selected from conductive abrasive grains and fired conductive abrasive grains exhibiting conductivity after firing in an atmosphere. It is configured. The inorganic abrasive grains 2 may contain non-conductive abrasive grains 5. This conductive whetstone 1 Is formed into a predetermined shape by a slurry casting method or a pressure forming method using a dispersion slurry containing inorganic abrasive grains 2, dried and then fired in a non-oxidizing atmosphere at 1000 to 2000 ° C. It is manufactured by It is preferable to add a dispersant or an organic binder which disappears by firing to the dispersion slurry. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2012124718-A1 |
priorityDate | 2002-01-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 32.