http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2003191313-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_24aca9ded2638ea793d05360dde7a4a0 |
classificationIPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29L7-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29K23-00 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C47-88 |
filingDate | 2001-12-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d4688b8289b284724e3fbfa816bacecf |
publicationDate | 2003-07-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2003191313-A |
titleOfInvention | Method for producing thermoplastic resin film |
abstract | PROBLEM TO BE SOLVED: To produce a thermoplastic resin film in which a molten film extruded from a lip of a T-die is drawn onto the chill roll while sucking air between the molten film and the chill roll, and cooled and solidified. A method for producing a thermoplastic resin film having an excellent balance of physical properties between MD and TD at a high speed. SOLUTION: In a method for producing a thermoplastic resin film, a molten film extruded from a lip of a T-die is drawn onto a chill roll while sucking air between the molten film and the chill roll, and cooled and solidified. The speed is 150-1000 m / min, and the temperature gradient of the MD of the film at the chill roll contact is 0.1-2. A method for producing a thermoplastic resin film having a temperature of 5 ° C./mm. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2006117898-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2007004324-A1 |
priorityDate | 2001-12-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 68.